Parts Management
1-4-132
Image File:
Process:
BRIGHT TIN 10 Minutes. 5 strings of 5 pieces. 1-1.5V and 20-25 amps for Tin Portion
Remarks:
Bright Tin over Electroless Nickel Base. Activate each string 3V in EN for 15 seconds. 5-10 Minute Nickel Base Plate (.00005)and 10 Minute Bright tin Plate (.0003). Neutralize after EN in anodize before Tin. DO NOT TOUCH BAR. Do Not go through anodize before Electroless Nickel. Only Hydrochloric Acids and appropriate rinses and pre-rinses.